Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Hangzhou Hengtong Metal Hose Co., Ltd. has produced mechanically formed stainless corrugated gas tube since 1990 and publishes the bend, support and coating data that keep these mechanisms from starting.
A corrugated gas hose stress corrosion cracking chloride cause prevention review begins by reading the crack, because chloride cracking, fatigue cracking and mechanical damage leave different evidence. The wrong diagnosis sends you to the wrong fix — re-torquing a fitting when the real problem is a collapsed corrugation, or specifying a thicker wall when the problem is a chloride source.
Chloride stress corrosion cracking needs three conditions at once: chloride ions, tensile stress, and temperature above roughly 50°C. Remove any one and the mechanism stops. This is the cause behind the uncoated stainless connector recalls of the 1980s and 1990s, and it is still the most misdiagnosed failure because it is invisible until the crack is through the wall. Even 316L is not immune in a hot chloride environment; where the exposure cannot be removed, a duplex grade or a intact protective jacket is the answer. Coastal atmospheres, pool chemicals, de-icing salts and some cleaning agents supply the ions — the hose rarely supplies them itself.
Fatigue is the second mechanism, and it is the one most often traced to installation. Bend a corrugated tube tighter than its minimum radius and the corrugation peaks flatten; the hose still holds gas and looks acceptable, but the collapsed section now carries permanent tensile stress. Pressure cycling, thermal movement and settlement work that section into a hairline crack. The symptom is frequently weeping at the fitting, which gets blamed on the fitting — the fitting is re-torqued, the crack remains, and the same failure repeats on the next unit.
Mechanical damage is the third category and the easiest to see once you know where to look. Rodent damage stainless steel Corrugated Hose outdoor protection matters in cable runs, crawl spaces and agricultural installations, where gnawing through a polyethylene jacket exposes the strip to the chlorides that then drive the first mechanism. Abrasion at a support point, a striker plate omitted on a concealed run, or a hose used as an earthing conductor all produce localised damage that starts as a coating breach and ends as a crack. The signature is a localised defect with clean metal on either side, often at a point where the jacket is scored or missing — quite different from the distributed fine cracking of chloride attack or the single hairline at an over-bent peak.
That distinction is practical: a single chewed section is a protection problem solved with conduit, while cracking across a heated coastal run is a chemistry problem solved with a barrier grade. Treating both as "a bad batch" wastes the evidence. This is why rodent damage stainless steel corrugated hose outdoor protection belongs in the specification for any exposed run rather than being left to the installer.
The three mechanisms share a supporting cast, and this is where the corrugated gas tubing support spacing hanger interval requirement earns its place in a failure review. A bend is only as good as the support around it: the bending moment at a curve is carried along the unsupported length, and every hanger too far apart adds load the bend must absorb. North American practice supports horizontal CSST runs every 4 to 6 ft and at every floor on vertical runs, deferring to the manufacturer's manual; European practice under BS 6891 and EN 1775 is the same in shape. Support spacing does not cause a crack by itself — it removes the margin that lets the tube survive one.
✅ Bottom line: Read the crack before naming the cause. Chloride cracking needs ions, stress and heat together; fatigue starts at an over-bent or re-bent section; mechanical damage starts at a breached jacket — and support spacing decides whether the tube can absorb any of them.
The controls that prevent these failures are all specifyable at the order stage, which is why a failure review should end in a purchase-order revision rather than a training reminder. Start with the coating: a listed CSST system uses a polyethylene jacket that is both a chloride barrier and, on leak-detection variants, permeable enough that a pressure drop registers through it. Specifying a bare tube for an outdoor or coastal run removes the first line of defence and should be an explicit decision, never a default.
For the fatigue mechanism, write the minimum bend radius per DN into the order alongside the straight-run requirement at the fitting and a prohibition on re-bending at the same point. Installers who receive those three numbers as a data sheet follow them; installers who receive only "flexible hose" improvise, and the improvisation is what fails in year three. Where vibration is present, specify isolating clamps or double-braid construction and bring the support interval down — a hose that is constantly moving needs more support, not less, and a fatigue crack is the consequence of getting that backwards.
Rodent damage stainless steel corrugated hose outdoor protection is handled at the same stage: specify a rodent-resistant jacket or a protective conduit for exposed runs, and require that any buried route use the conduit or engineered system the listing calls for rather than direct burial. A protective sleeve that is specified after a failure has already happened is a remediation, not a prevention, and it costs far more than the jacket upgrade at purchase.
HENGTONG supplies the corrugated gas tubing support spacing hanger interval requirement and bend data with every coil, and builds the RSB series with a yellow or transparent-yellow polyethylene jacket over mechanically formed 304 or 316L strip. Our tapered rigid-seal termination removes the gasket and the circumferential weld — two of the traditional weak points a failure review finds at the fitting. When a returned unit comes back, we look at the crack location, the jacket condition and the bend geometry together, because the answer is almost never a single cause.
Hangzhou Hengtong Metal Hose Co., Ltd. runs 6,000 m² with 10+ automated lines and 1,000+ tonnes of annual capacity, holds CSA, IAPMOF and ISO 9001/14001/45001 certification, and provides OEM and ODM supply to importers and distributors — matched fittings, custom lengths, coating options and private-label packing. Ask for the installation data sheet and we will flag the details that put a coating at risk.
✅ Bottom line: Prevent failure at the order stage — specify the jacket, the bend radius, the straight run, the support interval and the protection for exposed runs. A failure review that ends in a purchase-order revision has done its job.
Q: A hose failed after two years near an appliance. Is it the fitting or the tube? A: Check the bend first. A crack that starts just outside the bend and weeps at the fitting is the classic signature of an over-bent corrugation, not a faulty connector. Re-torquing the fitting will not stop it. A corrugated gas hose stress corrosion cracking chloride cause prevention check should also confirm the jacket is intact and the environment is not supplying chlorides.
Q: Does 316L eliminate chloride cracking? A: No. It raises resistance but does not remove the mechanism in a hot chloride environment with tensile stress. A corrugated gas hose stress corrosion cracking chloride cause prevention programme therefore treats grade as one control among several: if chlorides cannot be excluded, the answer is an intact barrier jacket, a duplex grade, or a change to the installation — not a grade substitution alone.
Q: How do I know whether support spacing contributed? A: Compare the installed hanger interval with the manufacturer's published figure for that DN and check whether any bend occurs close to an unsupported span. If the spacing is wide at a bend, load was transferred into the corrugation that the support should have carried — the corrugated gas tubing support spacing hanger interval requirement exists for exactly this reason.
Send us your DN size, installation environment, run length and destination market, and we will return the bend radius, support interval, jacket specification and protection recommendations, plus MOQ, lead time and a factory-direct price. HENGTONG supplies OEM and ODM corrugated stainless steel gas hose to importers and distributors — matched fittings, custom lengths, coating options and full batch documentation. Hangzhou Hengtong Metal Hose Co., Ltd. has produced corrugated gas hose since 1990. Ask for the data pack and we will flag the details that put a batch at risk.
Let's get in touch.
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.
Fill in more information so that we can get in touch with you faster
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.